(2) An in-situ blend method was used to prepared iPP/sPS alloys.
(2) 原位混合方法:将DQ催化剂制得的iPP溶于130℃十氢萘和苯乙烯单体中,加入催化剂Cp~*Ti(OMe)_3催化苯乙烯间规聚合,得到了iPP/sPS合金。
5 was prepared by using an in situ kneading drying calcination synthesis technique.
采用原位干混合煅烧合成法在钛合金基体上成功制备了K2Ti6O13涂层,并对涂层的微观形貌、相组成、涂层-基体的结合强度进行了研究,通过模拟体液实验对其生物活性进行了评估。
Styrene,surfactant and selected superabsorbent polymers were mixed and the in-situ blend polymerization of styrene was carried out when the initiator benzoperoxide was added.
采用乳液聚合法合成了一系列不同单体组成的高吸水树脂,选取吸水树脂与苯乙烯、表面活性剂组成聚合体系,用过氧化苯甲酰引发进行原位共混聚合,制备遇水崩解型聚苯乙烯,并考察了吸水树脂的种类、吸水倍率对崩解材料崩解性的影响。
Styrene, surfactant and superabsorbent polymers weremixed and the in-situ blend polymerization of styrene was carried out when theinitiator benzoperoxide was added.
将制备的吸水树脂与苯乙烯、表面活性剂(Span-80)组成聚合体系,用过氧化苯甲酰引发进行原位共混聚合,制得遇水崩解型聚苯乙烯。